paper · doi:10.1107/s0021889883011279
The title compound has been synthesized by sintering oxide mixtures between 1975 and 2175 K. It decomposes at or below ca 1875 K. Quenched to room temperature, the phase is trigonal with a o = 3.2496(1), c 0 = 25.221(1) Å, V = 230.65(2) Å 3 , Z = 1, D m = 3.95(1) g cm −3 , refraction indices ∊ D 293 K = 1.805(5), ω D 293 K = 1.855 (5) and birefringence Δ ′ = 0.05. The JCPDS File No. for magnesium aluminium zirconium oxide is 34-1495.