vix.ing · top · new · best · stats · spec

Naphthalene Diimide and Pyromellitic Diimide Networks as Cathode Materials in Lithium‐ion Batteries: on the Instability of Pyromellitic Diimide

2025/01/13 by Rukiya Matsidik, Daniele Fazzi, Andreas Seifert +1 · 1 voice
Chemical Engineering · Engineering · #Advanced Battery Materials and Technologies #Advancements in Battery Materials #Ionic liquids properties and applications

paper · pdf · doi:10.1002/marc.202401121

openalex publication_date 2025/01/13 · openalex created_date 2025/10/10 · openalex updated_date 2026/07/31

Abstract

Aromatic diimides such as naphthalene diimide (NDI) and pyromellitic diimide (MDI) are important building blocks for organic electrode materials. They feature a two-electron redox mechanism that allows for energy storage. Due to the smaller size of MDI compared to NDI its theoretical capacity is higher. Studies on MDI-based small molecule and linear polymer electrodes indicate that MDI is unstable, yet the origin of instability remains unclear. Herein, two cross-linked networks of NDI and MDI are designed. The polymers, termed PNDI-EG and PMDI-EG, are synthesized via cationic polymerization of vinyl ethylene glycol-functionalized NDI and MDI monomers. The cross-linked structures preclude extrinsic degradation pathways (e.g., dissolution in the electrolyte), and thereby facilitate the investigation of intrinsic degradation mechanisms. PMDI-EG-based cathodes are less stable, and the performance of PMDI-EG/Li half cells is markedly inferior compared to PNDI-EG/Li cells. Our comprehensive experimental and quantum-chemical investigation reveals that PMDI-EG undergoes irreversible diimide ring opening upon prolonged charge-discharge cycles, while PNDI-EG remains intact. It is hypothesized that the smaller ring size of the five-membered imide renders MDI more susceptible to side reactions with nucleophiles in the electrolyte, causing rapid loss of capacity during the first cycles.